EC-STM image of the transition from (2 x 3) to ( 3 x 3 ) on the unreconstructed Au(111) surface at -0.4 V vs. 3 M Ag/AgCl in 0.2 mM CdSO4 + 1 mM H2SO4. Image size is 3.5 µm x 3.5 µm.

Data Coutesy of Marcus D. Lay and John L. Stickney, Univ. of Georgia.

The 3D animation was rendered with the SPIP software.