Nanoscience Instruments

easyScan 2

curve

Back to Back to
Atomic Force Microscope Systems

All Products

 

The Nanosurf® EasyScan 2 Specifications

Electronics
 Electronics size / weight  470 x 120 x 80 mm / 2.4 kg
 Power Supply  90 - 240 V~/ 30 W  50 / 60 Hz
 Computer interface  USB 1.1
 Integrated USB hub  2 Ports (100 mA max)
 Measurement channels  16 bit A/D converters, up to seven signals depending on configuration
 Scan generator  16 bit D/A converter for all axes
 Scan speed  Up to 60ms / line at 128 datapoints / line
 Scan drive signals  ± 10 V, no high voltage!
 Scan area and data points  Individual width / height, up to 2048 x 2048 points
 Scan image rotation  0° - 360°
 Sample tilt compensation  Hardware X/Y-slope compensation
 Spectroscopy modes  Single point measurements or multiple measurements along a vector
 Spectroscopy measurement averaging  1-255
 Spectroscopy data points  Up to 2048
Adapters for former easyScan Scan Heads available
 
Software
 Various charts of the scan data can 
 be displayed simultaneously
 Line graph, Colour map, 3D view, ...
 Customizable display and parameter settings using user profiles
 On-line processing functions  Mean fit, Polynomial fit, Derived data, ...
 Quick evaluation functions  Distance, angles, cross-section, roughness, ...
 Data export  BMP, ASCII, CSV, ...
 Very easy installation
 
PC Requirements  (computer not included with system)
 Physical Type  Desktop or Laptop
 Operating System  Windows 2000, XP, Vista
 Minimum Hardware Recommendations  Pentium 4/M or AMD Athlon processor, 256MB RAM, True color 1024x768
 monitor, Hardware (HW) OpenGL graphics accelerator
 Data Port  USB port
 
Nanosurf easyScan 2 Scripiting Interface
 Applications  Automating measurement tasks, lithography, custom evaluation functions,  using third party measurement equipment
 Included control software  Windows Scripting Host: Visual Basic Script, Java Script, ...
 Remote controlled by  COM compatible languages: LabView, MathLab, Visual Basic, Delphi, C++...
 
 
Nanosurf easyScan 2 Signal Module: S
Available monitor signals  X-axis, Y-axis, Z-Axis, Approach, Tip Voltage, STM Current or AFM Deflection, Excitation, Amplitude, Phase
Full scale corresponds to  ± 10 V, Excitation: ± 5 V
Power supply output  GND, + 15 V,  - 15 V
 
Nanosurf easyScan 2 Signal Module: A
 All Signal Module S signals
 Additional signal modulation inputs  X-axis, Y-axis, Z-Axis, Tip voltage, Excitation
 Free connectors  2 x Aux, connection made on user request
 Modulation range  ± 10 V, Excitation: ± 5 V
 Additional analog user inputs  2 x 16 bit A/D, ± 10 V
 Additional analog user outputs  2 x 16 bit D/A, ± 10 V
 Synchronization output  1 x TTL: start, point sync pulses, variable width
 Additional modes  Almost unlimited
 User inputs can optionally be measured in all Imaging and Spectroscopy modes
 User outputs can be modulated in Spectroscopy measurements
 

STM Measurements

 STM Scan Head:  500nm  1µm  500 nmLC  1 µmLC
 Max. Scan range 1)  500 nm  1.0 µm  500 nm  1.0 µm
 Max. Z-range 1)  200 nm  200 nm  200 nm  200 nm
 Drive resolution Z 2)  3 pm  3 pm  3 pm  3 pm
 Drive resolution XY 2)  7.6 pm  15 pm  7.6 pm  15 pm
 Current set point  0.1 - 100 nA in 25 pA steps  0.2 - 20 nA in 5 pA steps
 
 Imaging modes  Constant Current (Topography), Constant Height (Current)
 Spectroscopy modes  Current-Voltage, Current-Distance 
 Tip voltage  ± 10 V in 5mV steps
Sample approach  Stick-slip motor
Sample size  Max 10 mm diameter
 
1) These are typical values
2) Calculated by dividing the maximum range by 16 bits; atomic resolution on HOPG can be obtained with all
   STMs
 
AFM Measurements
 AFM Scan Head:  10µm  70µm  110µm
 Maximum Scan range 1)  10 µm  70 µm  110 µm
 Maximum Z-range 1)  2 µm  14 µm  22 µm
 Drive resolution Z 2)  0.027 nm  0.21 nm  0.34 nm
 Drive resolution XY 2)  0.15 nm  1.1 nm  1.7 nm
 XY-Linearity Mean Error  < 0.6 %  < 1.2%  < 0.6%
 Z measurement noise level
 (RMS, Static Mode)
 0.07 nm
 (max. 0.2 nm)
 0.6 nm
 (max. 0.8 nm)
 0.4 nm
 (max. 0.55 nm)
 Z measurement noise level
 (RMS, Dynamic Mode)
 0.04 nm
 (max. 0.07 nm)
 0.5 nm
 (max. 0.8 nm)
 0.3 nm
 (max. 0.55 nm)
 
 Design  Tripod Stand-alone    Scan head weight  350 g
 Sample observation optics  Dual lens system  (top/side view)  Sample size  Unlimited
 Optical magnification  Top 12 x / Side 10 x  Automatic approach   5 mm
 View field  Top 4 x 4 mm / Side 5 x 3 mm  Max. approach speed   0.1 mm/s
 Sample illumination  White LEDs Cantilever alignment  Automatic adjustment
 Electrical connection to tip  Available    
 
1) Manufacturing tolerances are ± 15 % for 10 µm and 70 µm, ± 10 % for 110 µm scan heads
2) Calculated by dividing the maximum range by 16 bits
 
AFM Basic Module
 Imaging modes  Static Force (Contact), Const.Force (Topography), Const.Height  (Deflection)
 Spectroscopy modes  Force - Distance, Force - Tip voltage
 Tip voltage  ± 10 V in 5mV steps
 The AFM Basic Module is required for using AFM Scan Heads
 
AFM Dynamic Module
 Additional imaging modes  Dynamic Force (Intermittent Contact, etc.),
 Const. Amplitude (Topography), Const. Height (Amplitude)
 Additional spectroscopy modes  Amplitude - Distance
 Dynamic frequency range  15 - 300 kHz
 Dynamic frequency resolution  < 0.1 Hz
 The AFM Basic Module is required for using the Dynamic AFM Module
 
AFM Mode Extension Module
 Additional imaging modes  Phase Contrast, Force Modulation, Spreading Resistance
 Additional spectroscopy modes  Phase - Distance, Current - Voltage, Current - Distance, etc.
 Phase contrast range  ± 90°
 Phase contrast resolution  < 0.05°
 Phase reference range  0 - 360°
 Tip current measurement  ± 100 µA, 3 nA resolution
 Both the AFM Basic Module and the AFM Dynamic Module are required when using the AFM Mode Extension
 Module.
 
AFM Probes
 Manufacturer Compatibility  Applied Nanostructures, Vistaprobes™, Nanosensors and Nanoworld®
 Mode Compatibility  Static Force / Contact Mode,
 Dynamic Force / Tapping / Alternating Contact Mode,
 Spreading Resistance / Electrostatic Force Mode,
 Force Modulation Mode,
 Magnetic Force Mode
 Available Tip Types  Standard pyramidal, Rotated pyramidal, Super Sharp, High Aspect Ratio, Tipless
 Conducting, Magnetic, Diamond coated, and more
 Typical Load  10 nN
 Typical DFM frequency  190 kHz
 
Video Module
 Camera system  Dual video (top/side view)
 Magnification  Top 100 x / Side 70 x
 View Fields  Top 3.2 x 2.7 mm / Side 4.1 x 3.4 mm
 Image pixels  352 x 288
 Video display  In control software, can be saved as JPEG
 Analog video output  PAL Video-S
 
Micrometer Translation Stage
 XY resolution  < 0.5 µm
 Travel  13 mm
Specifications are subject to change without notice