Doped diamond probes offer a unique combination of unrivaled hardness and conductive properties. The tip side of these silicon probes is coated with polycrystalline diamond. The diamond is in-situ doped with boron to make it highly conductive. The reflex side of the cantilever is coated with Aluminum.