Electrospinning & Electrospraying Equipment

A full range of electrospinning machines to cover all needs at your lab

Contact

Compare Fluidnatek And Spinbox Products

Model

Spinbox

LE-50

LE-100

LE-500

Fluidnatek HT

  Spinbox electrospinning system Product Image of the Fluidnatek LE-50 Electrospinning Machine Product Image of the Fluidnatek LE-100 electrospinning machine Product Image of the Fluidnatek LE-500 Electrospinning Machine Product image of Fluidnatek HT Industrial Electrospinning Machine
Maximum sample size (mm) 200 x 314 200 x 314 300 x roll capacity 500 x roll capacity 1,600 x roll capacity
Maximum number of syringe pumps 3 2 3 3 N/A
Maximum number of needles 5 10 40 370 5,500+
Maximum voltage drop (kV) 40 40 60 80 120
Maximum volume per batch (mL) 420 280 420 8,000 50,000
Collector polarity Optional -10kV Optional -10kV Optional -30kV Standard -30kV Standard -60kV
Automatable axes 1 (Y) 2 (X,Y) 3 (X,Y,Z) 2 (Y,Z) 1 (X)
Metrology system No No Optional Optional Optional
Taylor cone visualization camera Optional Optional Optional Optional N/A
Ultraclean cabinet (HEPA/ULPA exhaust filtration) No Optional Optional Optional Optional
UV-C lamps No No Optional Optional Optional
Remote ethernet access No Yes Yes Yes Yes
Recipe-operated system No Optional Optional Optional Optional
Actively regulated exhaust No Optional Optional Standard Standard
Relative humidity & temperature conditioning No Optional Optional Optional Standard
Dimension, W x D x H (cm) 50 x 55 x 52 85 x 57 x 85 90 x 124 x 195 125 x 160 x 220 900 x 260 x 220 (HT)
300 x 150 x 200 (ECU)

Standard features on all models

Options available on all models

  • Adjustable target distance
  • LED lighting (to visualize sample processing)
  • Exhaust system
  • SS, Al and glass frame and enclosures
  • CE safety compliance
  • Needle translation (to obtain wider samples)
  • Multi-phase nozzle (co-axial)
  • Collectors:
    • Stationary (flat plate)
    • Rotating (disk, mandrel, drum)