Next Generation Nanofibers for Air Filtration

Aligned and Random Nanofibers

Originally Aired:

Date: May 12, 2020

Abstract:

Advanced Nanofiber Production with Disruptive Technologies: Precision Electrospinning with the Fluidnatek & fast analysis with the Phenom desktop SEM

As the demand for air filtration materials has increased globally, especially in the wake of an aerosol-based global pandemic, alternative sources of filter fibers are now an area of significant focus. Electrospun nanofiber filters represent a promising candidate due to the enhanced fine particle removal, versatile fiber functionalization, and ease of filter regeneration. However, to realize these properties, proper control over environmental conditions during electrospinning tethered to efficient and reliable methods for analyzing fiber structural properties are imperative.

We invite you to join application scientist James Stanfill from Nanoscience Instruments as he presents how the Fluidnatek electrospinning system and the Phenom desktop SEM offer the ultimate combined toolset for scaled production and structural analysis, respectively, of next-generation nanofiber-based air filtration materials.

In this webinar we will detail

  • Advantages of nanofibers for air filtration
  • “Perfect Nanofibers Every Time” with the Environmental Control Unit
  • Automated fiber and pore size analysis with the Phenom desktop SEM

Presentation By:

James Stanfill, PhD
Application Scientist
Nanoscience Instruments



Related Webinars:

Scanning Electron Microscopy

Practical SEM and Ion Mill Applications for Semiconductor R&D to Production

Scanning Electron Microscopes (SEMs) and Cross-sectioning/Polishing tools play a vital rol…

Scanning Electron Microscopy

Unlocking the Power of Desktop SEM for Pharmaceutical Development and Quality Control

As the pharmaceutical industry grows and new products are being researched and manufacture…

Scanning Electron Microscopy

Automating Battery Materials Analysis using Avizo Trueput with Phenom Desktop SEMs

Battery manufacturers face increasing demands for higher throughput, reproducible quality…

This site is protected by reCAPTCHA and the Google Privacy Policy and Terms of Service apply.